Guide ·

Aluminium Grades Explained: 5005, 5083, 6060 and 6061

By Shape Aluminium Ballina7 min read

Lengths of aluminium flat bar and round rod laid out on a workbench, ready to be measured and cut

Aluminium grades are four-digit numbers that name the alloy. The first digit tells you the main alloying element, and the letter and number after it (like H34 or T6) tell you how it was hardened. In our range: 5005 for sheet work, 5083 for boat and heavy plate, 6060 for everyday sections and 6061 for structural sections and plate.

The size tables in our catalogue list a grade and temper next to the sizes, such as “5005 H34” or “6061 T6”. This guide explains what those codes mean, compares the grades in our range in one chart, and shows which one suits the job you have in mind.

What do aluminium grade numbers mean?

Wrought aluminium (sheet, plate, bar and extrusions) uses an internationally registered four-digit designation. The first digit is the series, and it tells you the main element added to the aluminium; the full number names the particular alloy.

The series also tells you how the alloy gets its strength. Heat-treatable alloys are strengthened by heat treatment and ageing. Non-heat-treatable alloys get their strength from being rolled or worked (strain hardening), and heating them won’t make them stronger. The table follows the Australian Aluminium Council’s Rolled Products Manual.

SeriesMain alloying elementHeat-treatable?Grades in our range
1xxxNone (99% or purer aluminium)No–
2xxxCopperYes2011 machine rod
3xxxManganeseNo (generally)3003 propeller plate
4xxxSiliconMostly not; used mainly for welding wire–
5xxxMagnesiumNo5005 sheet, 5052/5251 treadplate, 5083 plate
6xxxMagnesium and siliconYes6060, 6061, 6063, 6106 and 6005A sections, 6061 plate
7xxxZinc (with magnesium)Yes–

Almost everything in our catalogue is 5xxx (sheet and plate) or 6xxx (extruded sections like angle, channel and tube).

What do aluminium temper codes like H34 and T6 mean?

The temper is the letter and number after the grade. It tells you how the metal was treated, which changes how strong and how bendable it is. An H means strain hardened (non-heat-treatable grades). A T means heat treated. An O means annealed, the softest condition, and F means as fabricated, with no strength limits.

TemperWhere you’ll see itWhat it means in plain words
H345005 sheetH3 is strain hardened then stabilised (used only on magnesium-containing alloys); the 4 means half-hard.
H223003 propeller plateH2 is strain hardened then partly annealed; the 2 means quarter-hard.
H1165083 plate up to 8 mmA special temper used on 5083, made to resist stress-corrosion cracking and exfoliation, and checked by exfoliation testing.
H1125083 plate over 8 mmNo special control of the strain hardening or heat treatment, but minimum strengths still apply.
T32011 machine rod, 10 to 38.1 mmSolution heat treated, cold worked, then naturally aged.
T56060, 6063 and 6005A sectionsCooled straight from the extrusion press, then artificially aged (baked) to add strength.
T66061 and 6106 sections, 6060 telescopic tube, 2011 rod 39 mm and overSolution heat treated (or cooled from the press), then artificially aged.
T82011 machine rod, 6 to 9 mmSolution heat treated, cold worked, then artificially aged.
T6516061 plateT6, plus “51”: stress relieved by stretching (1.5 to 3% for plate).

You may also see extra digits, like the T594 on our 6063 rope section. These mark a variation of the basic temper.

Aluminium grades chart: how do the grades in our range compare?

This chart covers the grades in our catalogue. Strengths for sheet and plate are the minimums in the Australian Aluminium Council’s Rolled Products Manual for the temper and thickness shown (tensile, then yield, in MPa; the manual notes some yield figures aren’t guaranteed unless requested). The manual covers sheet and plate only, so we don’t quote figures for extruded sections here: ask us, or your engineer, for the section you’re using.

Grade and temperIn our catalogue asMin. tensile / yield (MPa)What the Council says
3003 H22Propeller plateNot listed3000 series: chemical equipment and sheet metal work.
5005 H34Sheet135–180 / 105 (1.3–3 mm)Sheet metal work and small boats; good resistance in marine atmospheres.
5052 / 5251 (temper not listed in our catalogue)TreadplateFor reference, 5052 H32 sheet: 215–265 / 160Sheet metal work and small boats; the original “marine grade” alloys.
5083 H116 / H112Plate305 / 215 (H116, 1.6–12.5 mm); 275 / 125 (H112, 6–12.5 mm)Marine, road transport and general plate; good welding characteristics.
6061 T6 / T651Plate; structural angle, channel, bar and round tube290 / 240 (T6 sheet and plate, 0.5–12 mm)6000 series: heat-treatable, good formability and corrosion resistance.
6060 T5 / 6063 T5Angle, channel, tee, flat and square bar, round rod, tube; tray sectionsExtrusion standard6060 T5 has the same guaranteed minimums as 6063 T5.
6106 T6, 6005A T5Tray sections; planks and structural tubeExtrusion standard6000 series: medium strength, good corrosion resistance.
2011 T3 / T6 / T8Machine rodNot listed2000 series: copper alloys with lower corrosion resistance than most aluminium; can suffer intergranular corrosion.

What grade aluminium should you use for your job?

Here’s how the grades in our range line up with common jobs.

Ute trays and trailers

Our ute and trailer tray sections come in 6063 T5 and 6106 T6. For the frame of a trailer, our structural angle and channel are 6061 T6. Deck it with 5005 sheet or treadplate. The Council lists 5083 plate for road transport too, if the deck needs to be heavier.

Boats

Use 5000-series sheet and plate. The Council lists 5005, 5251 and 5052 for small boats and 5083 for marine plate, and the H116 temper of 5083 is made to resist exfoliation. For more on salt air and sea water, see our guide to whether aluminium rusts.

Signage, cladding and folded sheet work

5005 H34 is our standard sheet grade, listed by the Council for sheet metal work. If a part needs a tight fold, ask for the bend you need: harder tempers need a bigger bend radius to avoid cracking. See our sheet and plate range.

Brackets, frames, balustrades and gates

For light brackets, frames, railings and fences, our 6060 T5 angle, channel and tube is the everyday choice. Step up to the 6061 T6 structural sections when the part carries real load. A balustrade has to meet the National Construction Code, so take the sizes from your builder or engineer.

Machined parts

For turned parts on a lathe, we stock 2011 machine rod; give it a protective finish if it will see salt water. For milled parts cut from plate, 6061 T651 has been stress relieved by stretching.

Cool rooms

The cool room sections in our catalogue are all 6060 T5, in 6.5 m lengths. Start with the profile, not the grade: bring the panel thickness and system you’re working with and we’ll check which sections suit.

What mistakes do people make with aluminium grades?

  1. Bending 6061 T6 too tight. The Council’s minimum bend radii for 6061 T6 grow with thickness: about 1 times the thickness for thin sheet, 2.5 times at 3 mm, 4 times at 6 mm and 5 times at 12 mm plate. Tighter than that, the outside of the bend can crack. Use a generous radius, or ask about a softer temper for folded parts.
  2. Using 2011 where it gets wet. It’s a 2000-series copper alloy, with lower corrosion resistance than most aluminium. Keep it for parts that stay dry or get a protective finish.
  3. Trying to heat treat 5083. The 5000 series isn’t heat-treatable. Its strength comes from strain hardening, and heat won’t add any.
  4. Using the wrong filler wire. The Council’s manual uses 5356 (or 5183, 5556 or 5554) for 5000-series sheet and plate. 4043 can weld 5005 sheet but not the higher-magnesium alloys like 5083.
  5. Treating 6060 and 6061 as the same thing. They look the same on the rack, but 6061 T6 is our structural grade. Check the grade on the size table.

The short version: pick 5xxx when the job needs bending or sea water, 6061 when it needs strength, 6060 for everyday frames and trim, and 2011 only for parts you’ll machine. If you’re not sure, bring your drawing or the old part to the shed and we’ll talk it through and cut your lengths to size.

Frequently asked questions

What is the difference between 6060 and 6061 aluminium?

Both are heat-treatable 6000-series grades. In our range, 6061 T6 is the structural grade (structural angle, channel, bar, round tube and plate), and 6060 T5 covers everyday angle, channel, tee, flat bar, rod and tube. Check the grade on the size table.

What grade of aluminium is best for boats?

A 5000-series grade. The Australian Aluminium Council lists 5005, 5251 and 5052 for small boats and 5083 for marine plate; the H116 temper of 5083 is made to resist exfoliation.

Can you bend 6061 T6 aluminium?

Yes, with a generous radius. The Council’s minimum bend radii for 6061 T6 run from about 1 times the thickness for thin sheet to 2.5 times at 3 mm, 4 times at 6 mm and 5 times at 12 mm plate.

What does T6 mean on aluminium?

T6 means solution heat treated (or cooled from the extrusion press) and then artificially aged to make it stronger. You’ll see it on heat-treatable grades like 6061 and 6106.

Is 5083 aluminium heat-treatable?

No. The 5000 series is non-heat-treatable: 5083 gets its strength from strain hardening, so heating it won’t make it stronger.

What does H34 mean on 5005 sheet?

H3 means strain hardened and then stabilised, a treatment used only on magnesium-containing alloys, and the 4 means half-hard.

Sources

Written by

The team at Shape Aluminium Ballina

Shape Aluminium Ballina is Ballina’s local aluminium supplier: sheet, plate, angle, bar and tube in stock and cut to size, for trade and the public. These guides answer the questions we hear at the counter. About us

Get a quote

Need it cut to size?

Send your sizes and we’ll check the rack and cut it at the shed, ready to collect in Ballina or deliver locally.

From the shed

More guides

View all guides